MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ LUX2289 PC (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN LUX2289 resin is an injection molding grade with high light reflectance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Density 1.31 g/ccISO 1183
Water Absorption 0.35 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 17 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 61.0 MPa50 mm/min; ASTM D638
 62.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; ASTM D638
 61.0 MPa50 mm/min; ISO 527
Elongation at Break 120 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Flexural Strength 70.0 MPaISO 178
Flexural Yield Strength 98.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2500 MPaISO 178
 2670 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 648 J/mASTM D256
 165 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 2130 J/mASTM D4812
Izod Impact, Notched (ISO) 52.0 kJ/m²80*10*3; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 170 kJ/m²80*10*4; ISO 180/1U
 160 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched 140 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eU
 140 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 67.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 69.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 123 °C
@Treatment Temp. 120 °C,
Time 7200 sec
annealed; ISO 75/Ae
Vicat Softening Point 142 °CRate B/50; ASTM D1525
 144 °CRate A/50; ISO 306
 145 °CRate B/50; ISO 306
Flammability, UL94 HB
@Thickness 1.00 mm
UL 94
 V-2
@Thickness 1.50 mm
UL 94
Glow Wire Test 850 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 270 - 295 °C
Zone 3 280 - 305 °C
Melt Temperature 280 - 305 °C
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10502 / 243969

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.