MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds Smooth-Cast® 380 High Density Urethane Tooling Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Smooth-Cast™ 380 is a filled, high density casting resin formulated for a variety of tooling applications. This no-odor resin features a convenient 1A:1B mix ratio by volume, a 6 minute pot-life and cure time of about 60 minutes depending on mass and temperature. Low viscosity ensures minimal bubble entrapment and long term shrinkage of cured resin is very low. Cured material is very strong can be machined, drilled, sanded, etc. Color can be added with SO-Strong™ color tints.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/ccASTM D-1475
Viscosity 1140 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0025 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ASTM D-2240
Tensile Strength, Ultimate 3550 psiASTM D-638
Elongation at Break 1.43 %ASTM D-638
Tensile Modulus 490000 psiASTM D-638
Flexural Strength 4870 psiASTM D-790
Flexural Modulus 315000 psiASTM D-790
Compressive Strength 7860 psiASTM D-695
Compressive Modulus 126000 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 53.0 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 minHandling Time
Pot Life 6.00 minASTM D-2471
 
Descriptive Properties
ColorTan
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume15.9[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN027 / 296728

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.