Description: Epoxy structural tackifier in 400ml spray too be sprayed on fabrics and tools to improve tackiness at room temperature and help operators laying up preforms. Features: HexBond™ ST1153 is compatible with most epoxy prepregs and epoxy resins curing at 180°C/356°F without any degradation of final mechanical properties. Once the solvent is evaporated, HexBond™ ST1153 sets and is non-tacky. This provides a high-strength “assembly”. Information provided by Hexcel Corporation. |