MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips 7109BK Linear low density polyethylene blown film resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109

Characteristics: good stiffness at thin gauges, good drawdown, low COF, can be used straight or blended with LDPE or HDPE

Applications: industrial liners, garment bags, carrier bags, coextrusions

Natural Color. 1000 ppm Slip. 5000 ppm Antiblock.

Film properties below based on thickness of 0.0318 mm. Extruder 6.35 cm. Screw L/D ratio 24:1. Die opening 0.1905 cm. Blow-Up Ratio 2:1.

Information provided by Chevron Phillips Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D4833-89
Melt Flow 0.90 g/10 min0.90 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 640 %640 %ASTM D882
Secant Modulus, MD 0.255 GPa37.0 ksiASTM D882
Secant Modulus, TD 0.337 GPa48.9 ksiASTM D882
Coefficient of Friction 0.200.20ASTM D1894
Elmendorf Tear Strength, MD 16.5 g/micron419 g/milOrientation not specified; ASTM D1922
Elmendorf Tear Strength, TD 37.8 g/micron960 g/milASTM D1922
Dart Drop 4.10 g/micron104 g/milF-50 at 26 in.; ASTM D1709
Dart Drop Test 130 g0.287 lbF-50 at 26 in.; ASTM D1709
Film Tensile Strength at Break, MD 40.8 MPa5920 psiASTM D882
Film Tensile Strength at Break, TD 26.5 MPa3840 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D2457
Gloss 50 %50 %45°, ASTM D 2457
 90 %90 %60°, ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVVF8 / 20550

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.