Varcum 29109 is a thermosetting phenolic resin in lump form. APPLICATION: Varcum 29109 is recommended for use in metal coating applications. FEATURES: The use of modifying agents tend to reduce the maximum chemical resistance and, therefore, the incorporation of such agents is not generally recommended. Alcohol and/or ketone solvent systems are required with this product; the use of hydrocarbon solvents is not pratical. Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |