MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Extra-high-leaded brass, UNS C35600, H04 sheet/strip
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Fabricated by blanking, machining, piercing and punching, stamping.

Applications: clock plates and nuts, clock and watch backs, clock gears and wheels, channel plates.

Test specimen: sheet and strip - 1mm thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080
Hardness, Rockwell 30T 6969
Tensile Strength, Ultimate 510 MPa74000 psi
Tensile Strength, Yield 415 MPa
@Strain 0.5 %
60200 psi
@Strain 0.5 %
Elongation at Break 7.0 %7.0 %In 50 mm
Modulus of Elasticity 97.0 GPa14100 ksi
Poissons Ratio 0.3110.311
Machinability 100 %100 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 37.0 GPa5370 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
0.00000660 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.5 µm/m-°C
@Temperature 20.0 - 300 °C
11.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
798 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 885 - 905 °C1630 - 1660 °F
Solidus 885 °C1630 °F
Liquidus 905 °C1660 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 700 - 800 °C1290 - 1470 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 64.5 %59 - 64.5 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb 2.0 - 3.0 %2.0 - 3.0 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 34.5 %34.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-leaded brass, 62%, UNS C35300
High-leaded brass, UNS C34200, H06 Temper flat products
Medium-leaded brass, UNS C34000, H06 Temper flat products
Copper, UNS C26800 (Yellow brass), H04 Temper flat products
Copper, UNS C27000 (Yellow brass), OSO70 Temper flat products

MC35600b5 / 11237

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.