Electrically conductive silicone rubber for press molding, which are peroxide curing. Properties: ELASTOSIL® R 570/60 is not suitable for vulcanization using crosslinker E. The materials are black. Special features: - good mechanical and electrical properties
- high conductivity
- low volume resistivity
- good heat resistance
- good rheological properties
- combustion products of low toxicity and corrosivity and low smoke density
Application: Control elements for cable accessories, contacts and keypads, interconnectors, electrically conductive rollers, electrodes..Information provided by Wacker Chemie AG. |