MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Alcoa KAMA 5100 CPET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Capabilities
  • Gauge: .020" to .040" (508 to 106µm)
  • Width: 20" to 52" (508 to 1321mm)
  • Core size: 3" or 6"
  • Roll O.D.: 29" standard, available up to 40"
  • Silicone coating available
  • Available in natural black

Properties

  • Excellent for dual-ovenable applications
  • Good impact performance
  • Ideal for home meal replacement applications
  • FDA compliant to CFR 21 #177.1630
  • Kosher material

Information provided by Alcoa Kama Co.

Key Words: FDA Compliant: CFR 21 #177.1630
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/cc
Viscosity Measurement 0.78 - 0.850.78 - 0.85Intrinsic Viscosity; ASTM D3835
Thickness 508 - 1020 microns20.0 - 40.0 mil
Linear Mold Shrinkage 0.010 - 0.018 cm/cm0.010 - 0.018 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.5 - 62.1 MPa5000 - 9000 psiASTM D638
Elongation at Break 100 - 400 %100 - 400 %ASTM D638
Flexural Modulus 2.07 - 2.76 GPa300 - 400 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -12.2 °C10.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 160 °C280 - 320 °FThermoforming Temp
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Resistance to AcidGood to Excellent
Resistance to AlcoholsGood to Excellent
Resistance to AlkalisFair to Good
Resistance to Fat, Grease, and OilGood to Excellent
Resistance to Hydrocarbon SolventsGood to Excellent
Resistance to Strong OxidizersGood to Excellent
Yield, in²/lb/mil20810

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman VersaTray 12822 Plastic
Ex-Tech Plastics VersaTech™ APET
Alcoa KAMA 4100 Prime APET

PKAMA23 / 48679

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.