MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Geniosil® XB 502 Binder
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: GENIOSIL® XB 502 is a silane-terminated binder based on alpha-silane technology for the formulation of high-strength adhesives.

Alphasilane-terminated polyethers are an important group of moisture-curing binders that can crosslink without a tin catalyst. GENIOSIL® XB 502 is a transparent low-viscosity binder. The resultant adhesives display hardnesses in the high Shore D range when cured. This new polymer therefore represents an extension of elastic binders such as GENIOSIL® STP-E10 and can be mixed with this product group in any proportions in order to tailor the properties to the respective application.
Catalysts: Curing of GENIOSIL® XB 502 requires a catalyst that does not necessarily have to be organo-metallic. However dioctyl tin (e.g. TibKat 223) may be used if required. Catalysis can also be accelerated with titanium systems (Tyzor®TnBT or Tyzor® PITA-SM), as well as inorganic (phosphoric) or organic (tartaric) acids. Manufacturer recommends using an amine catalyst, and adjusting the skin-formation time by varying the amount of aminosilane used. GENIOSIL® GF 9 and GENIOSIL® GF 95 have proven particularly advantageous here. GENIOSIL® GF 95 can achieve improved water resistance, which is increased by the addition of epoxy silanes.
Plasticizers: A plasticizer can be used with the new binder, but impairs its mechanical properties. For example, GENIOSIL® XB 502 can be readily mixed with polyethers, phthalates, trimelletates and phosphoric acid ester. Another way of elastifying a GENIOSIL® XB 502- Based formulation is to use silane-modified polymers of the hybrid series GENIOSIL® STP-E. Tailored elastic adhesives can be developed while retaining the high strength properties.
Fillers: GENIOSIL® XB 502 can be formulated with a variety of fillers, in amounts of up to 70%. The range starts with oxidic materials, such as aluminum trihydroxide (e.g. Martinal® OL 104), quartz flours (e.g. Millisil® W10) or pyrogenic silicas (HDK® H13L), and extends to coated (Omyabond® 520, Hakuneka®CCR-S10) and uncoated chalks (Omyacarb® 5 GU). Based on a model formulation of 1:1 filler to GENIOSIL® XB 502 plus 1.5% GENIOSIL® GF 9 as the catalyst, tensile lap-shear strength values from 9 to 15 N/mm² with beech/beech test specimens were determined.
Stabilizers: Because of its polymer backbone, GENIOSIL® XB 502 is already stable to heat and light. However, manufacturer recommends using the conventional stabilizers employed in STP-E technology to guarantee long-time stability of the adhesive. Experiments have shown that a sterically hindered amine (e.g. Tinuvin 123) and an oxalanilide (e.g. Hostavin 3206) provide adequate stabilization.

Special features: Properties of the binder GENIOSIL® XB 502:

  • low viscosity
  • easy handling and dosing
  • tin-free catalysis
  • non-labeling
Properties of the formulated adhesive:
  • high mechanical strength with ast strength build up
  • hardnesses in the Shore D range
  • good adhesion to metals, glass and ceramics
  • non-bubbling
  • isocyanate,- tin- and solvent-free
  • good heat-stability
  • low yellowing tendency
  • formulation of water resistant products possible (D1 - D4)
Application: Adhesives can be formulated having high tensile lap shear strength (= 15 N/mm²) on a wide variety of substrates. With certain substrates, it may be advisable to modify the elasticity of the binder. Based on the model formulation and filler (1 : 1), with 2.5% GENIOSIL® GF 9 as catalyst, the tensile lap-shear strength of beech/beech and aluminum/aluminum test specimens was determined. While GENIOSIL® XB 502 is ideal for bonding wood, metals can be very readily bonded when GENIOSIL® XB 502 is mixed with GENIOSIL® STP-E10 in a ratio of 3 : 1.

Further state-of-the art bonding:

  • wood
  • stone
  • metal
  • ceramics
  • bonding of different substrates (e.g. wood/metal, metal/concrete)

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc
@Pressure 0.1013 MPa
0.0408 lb/in³
@Pressure 14.69 psi
DIN 51757
Viscosity 1300 cP1300 cPdynamic; DIN 51562
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °FISO 2719
Ignition Temperature 380 °C716 °Fliquids; DIN 51794
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear
Color<50Hazen color index, DIN ISO 6271

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nabaltec APYRAL® 120E Al(OH)3
Indium Corp. Indalloy 12 Lead Solder Alloy
Wacker Geniosil® STP-E 10 Hybrid Polymer
Omya OMYACARB® UF - FL Calcium Carbonate
Omya OMYACARB® F - FL Calcium Carbonate

PWACK9331 / 204860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.