MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EMS-Grivory Grilon® FG 40 NL nat 6025 Nylon 6, Nucleating Agent, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Nucleated

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Nucleating Agent; UV Stabilizer

Features: Barrier Resin; Food Contact Acceptable; High Viscosity; Medium Viscosity; Nucleated

Uses: Cast Film; Coating Applications; Film; Medical Packaging; Non-oriented Film; Oriented Film; Packaging; Paper Coatings; Tubing

Agency Ratings: EU Food Contact; FDA Food Contact

RoSH Compliance: RoSH Compliant

Appearance: Natural Color

Forms: Granules

Processing Method: Blown Film; Cast Film; Extrusion; Film Extrusion

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption 3.0 %3.0 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 9.0 %9.0 %ISO 62
Water Vapor Transmission 10.1 g/m²/day0.650 g/100 in²/day85% RH; ISO 15106-1/-2
Oxygen Transmission 25.0 cc-mm/m²-24hr-atm63.5 cc-mil/100 in²-24hr-atm0% RH; ISO 15105-1/2
 30.0 cc-mm/m²-24hr-atm76.2 cc-mil/100 in²-24hr-atm85% RH; ISO 15105-1/2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm203 cc-mil/100 in²-24hr-atm0% RH; ISO 15105-1/2
 150 cc-mm/m²-24hr-atm381 cc-mil/100 in²-24hr-atm85% RH; ISO 15105-1/2
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 275 °C
20 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 40.0 MPa5800 psiISO 527-3
Film Tensile Strength at Yield, TD 40.0 MPa5800 psiISO 527-3
Film Elongation at Break, MD 600 %600 %ISO 527-3
Film Elongation at Break, TD 900 %900 %ISO 527-3
Film Elongation at Yield, MD 10 %10 %ISO 527-3
Film Elongation at Yield, TD 7.0 %7.0 %ISO 527-3
Tensile Modulus 3.00 GPa435 ksiISO 527-1
Coefficient of Friction, Dynamic 0.300.30ISO 8295
Tear Strength Test 286286[lbf/in], Trouser, MD; ISO 6383-1
 286286[lbf/in], Trouser, TD; ISO 6383-1
Elmendorf Tear Strength MD 1540 g1540 gISO 6383-2
Elmendorf Tear Strength TD 1540 g1540 gISO 6383-2
Film Tensile Strength at Break, MD 100 MPa14500 psiISO 527-3
Film Tensile Strength at Break, TD 90.3 MPa13100 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10ºC/min; ISO 11357-3
 
Optical PropertiesMetricEnglishComments
Gloss 100 %100 %60°; ISO 2813

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM497 / 307856

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.