Product Description: ENGAGE™ 8137 Polyolefin Elastomer is an ethylene-butene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in processing and makes ENGAGE™ 8137 highly effective as an impact modifier in polyolefin or as a component in injection molding applications. Main Characteristics: - Pellet form
- Low density
- Excellent flow characteristics
- Toughness, flexibility
Applications: - Injection molded industrial and consumer durable goods
- Impact modification
Availability: Asia Pacific; Europe; Latin America; North America Form: Pellets Information provided by The Dow Chemical Company |