MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QSil 550F Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 550F is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairable.

Key Features:

  • 100% solids
  • Fast gel time
  • Good elongation
  • Low modulus

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccUncatalyzed, QSil 255F A
 1.39 g/ccUncatalyzed, QSil 255F B
Viscosity 3500 cPUncatalyzed, QSil 255F A
 3500 cPUncatalyzed, QSil 255F B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60Cure 7 minutes at 150°C
Tensile Strength 611 psiCure 7 minutes at 150°C
Elongation at Break 112 %Cure 7 minutes at 150°C
Tear Strength 25.0 pliCure 7 minutes at 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.47e+15 ohm-cm
Dielectric Constant 3.12
@Frequency 1000 Hz
Dissipation Factor 0.0030
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.370 W/m-K
Maximum Service Temperature, Air 204 °CCured 7 minutes @ 150°C
Minimum Service Temperature, Air -55.0 °CCured 7 minutes @ 150°C
Flammability, UL94 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 min
@Temperature 150 °C
As Tested
Gel Time 7.00 minCatalyzed
 
Descriptive Properties
ColorBeige/WhiteUncatalyzed, QSil 255F A
 BlackUncatalyzed, QSil 255F B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PACC2092 / 199480

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.