KEBAFLEX / U A 90 ST B01 is a TPU with a Shore hardness of A 90. It is characterized by high flexibility and very good wear and abrasion resistance. Properties: flexible, good gliding properties, good recovery behavior, High wear resistance, impact resistant Information provided by BARLOG plastics GmbH. |