MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals Arcel 730 LV Resin 70% Polystyrene/30% Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: ARCEL advanced foam resin consists of polystyrene and polyethylene. ARCEL resin providesl toughness, flexibility and durability in a lightweight foam.

The strength and flexibility of ARCEL resin creates a resilient foam that can be molded into numerous complex and intricate forms. Its lightweight construction is resistant to puncture, flaking, tearing and breaking. In addition, packaging molded with ARCEL resin provides good cushioning and easy handling, while its lightweight properties help lower freight and other packaging costs.

ARCEL resin is available in low-pentane (LV) grades for customers governed by strict pentane emission laws or high-density applications.

Arcel 730 LV resin can be continuously or batch expanded using conventional EPS expansion equipment. Some minor material handling modifications may be required. For molded part densities below 32 g/L (2.0 pcf), double-pass expansion will be required to attain desired bulk densities.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0272 g/cc0.000983 lb/in³Expectation from Double Pass Expansion
 0.0288 g/cc0.00104 lb/in³Expectation from Batch Expansion
 0.0320 g/cc0.00116 lb/in³Expectation from Single Pass Expansion
Volatiles 8.5 %8.5 %Average VOC Content
Particle Size 800 - 1700 µm800 - 1700 µm98% within range
 
Descriptive Properties
ColorNatural (white)
ShapeSpherical
StorageMax. 4°C (40°F)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Peripor® 200 Expandable Polystyrene
NOVA Chemicals ARCEL® 730 Expanded Polyethylene/Styrenic Polymer
Overview of materials for Expanded Polystyrene (EPS)
NOVA Chemicals Styrocell® D733A Expandable Polystyrene
Ineos Nova T243C Expandable Polystyrene

PNOV790 / 108894

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.