MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Chemicals SOLKANE® 141b Surface Treatment Agent
Categories: Fluid

Material Notes: SOLKANE® 141b is a colourless liquid, with a slight ethereal odor, characterized by a high degree of chemical and thermal stability. SOLKANE® 141b is also quite stable when used in combination with ultrasonics, which can improve its cleaning efficiency if necessary.

CAS-No.: 1717-00-6 / EC-No.: 404-080-1 / Index-No.: 602-084-00-X /REACH Registration Number: 01-0000015369-63

Uses: Surface treatment agents

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 116.9 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point -103.5 °C
Boiling Point 32.0 °C
 
Descriptive Properties
AppearanceVolatile., liquid
Colorcolorless
Composition>99%1,1-Dichloro-1-fluoroethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6061A Composition Spec
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
Aluminum 6061-T913
Aluminum 6061-T8
Alclad Aluminum 6061-T6, T651

WSOLV082 / 147731

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.