MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Powersil® 570 Plus Silicone Insulator Coating
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 570 PLUS is a curable one-component silicon-in-water-emulsion.

Spray application forms a wet layer that dries and cures to a high voltage insulator coating with excellent electrical properties.

Special features:

  • Does not contain solvents
  • Ready-to-use
  • Primerless adhesion to selected substrates
  • Good resistance to weathering
  • Excellent hydrophobic properties
Application: A film of POWERSIL® 570 PLUS is applied onto porcelain or glass insulators as well onto the porcelain or glass surface of other high-voltage insulating equipment where surface contamination causes service problems. POWERSIL® 570 PLUS forms a long-term hydrophobic surface. Thus the formation of wet conductive layers is prevented, the electrical leakage current is minimized and the risk of pollution flashovers is eliminated.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³paste like; ISO 2781
 1.10 g/cc0.0397 lb/in³solid state; ISO 2781
Viscosity 1100 cP1100 cP100% deformation
 350000 cP350000 cP0.1% deformation
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 5.00e+15 ohm-cm>= 5.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.9
@Frequency 50 Hz
2.9
@Frequency 50 Hz
IEC 60250
Dielectric Strength <= 28.0 kV/mm<= 711 kV/inIEC 60243
 
Processing PropertiesMetricEnglishComments
Dry Time 6.00 hour
@Temperature 23.0 °C
6.00 hour
@Temperature 73.4 °F
50% RH
 
Descriptive Properties
Colorlight gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Powersil® 79032 Silicone Dispersion
Wacker Powersil® 567 Silicone Insulator Coating
Wacker Powersil® 555 R Silicone Dispersion
Wacker Powersil® 552 Silicone Insulator Coating

PWACK9376 / 204905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.