MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Ceramics ECO-1200A Alumina-Silica Insulation
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.310 g/cc
Loss On Ignition 5.0 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000660 GPaAs Received, Parallel to thickness
 0.000230 GPa
@Temperature 760 °C,
Time 86400 sec
Parallel to Thickness
Compressive Yield Strength 0.170 MPaat 10% Compression, Parallel to thickness
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 27.0 V/mil
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0550 W/m-K
@Temperature 200 °C
Parallel to Thickness
 0.0550 W/m-K
@Temperature 200 °C
 0.110 W/m-K
@Temperature 600 °C
 0.205 W/m-K
@Temperature 1000 °C
Parallel to Thickness
Maximum Service Temperature, Air 1200 °C
Shrinkage 0.50 %
@Temperature 760 °C,
Time 86400 sec
Perpendicular to Thickness
 2.5 %
@Temperature 1000 °C,
Time 86400 sec
Parallel to Thickness
 3.5 %
@Temperature 1000 °C,
Time 86400 sec
Perpendicular to Thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 33 %
Other 1.0 %Other Metal Oxides
 5.0 %Organic Content
SiO2 61 %
 
Descriptive Properties
ColorOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics ECO-1200B Alumina-Silica Insulation
Overview of materials for Silicone Polyurethane, Ether Based
Overview of materials for Silicone Foam
Overview of materials for Silicone Elastomer, for Thermal Management
Overview of materials for Liquid Silicone Rubber

CZIR036 / 2844

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.