System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate
Categories:
Polymer
;
Thermoplastic
;
ASA Polymer
;
Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Material Notes:
SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.
Information provided by SAX Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.07
g/cc
Linear Mold Shrinkage
0.0040
-
0.0070
cm/cm
Melt Flow
11
g/10 min
@Load 10.0 kg,
Temperature 220 °C
from MVR; ISO 1033
Mechanical Properties
Original Value
Comments
Tensile Strength
58.0
MPa
ISO 527-1
Elongation at Break
20 %
ISO 527-1
Tensile Modulus
2800
MPa
ISO 527-1
Izod Impact, Notched (ISO)
5.00
kJ/m²
@Temperature -30.0 °C
ISO 180/1A
8.00
kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO)
40.0
kJ/m²
@Temperature -30.0 °C
ISO 180
80.0
kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched
60.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
100
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched
5.00
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
7.00
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Thermal Properties
Original Value
Comments
Hot Ball Pressure Test
95.0
°C
@Thickness 2.00 mm
IE/CEN 60335-1
Deflection Temperature at 1.8 MPa (264 psi)
96.0
°C
80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point
110
°C
50B; ISO 306
Glow Wire Flammability Index
750
°C
IEC 60695-2-12
Processing Properties
Original Value
Comments
Melt Temperature
220
-
260
°C
Mold Temperature
60.0
-
90.0
°C
Drying Temperature
80.0
°C
@Time 7200 - 21600 sec
Moisture Content
<= 0.20 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® WR-9750H ASA, Unreinforced Extrusion Grade
A. Schulman Diamond DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
INEOS Styrolution Luran® S 797SE Q440 Acrylonitrile Styrene Acrylate (ASA)
INEOS Styrolution Luran® S KR2858 G3 Acrylonitrile Styrene Acrylate (ASA)
Lotte Advanced Materials Starex® WR-9310 ASA, Unreinforced Heat Resistant
PSAXP966 / 150915
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.