MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals DHJ-5
Categories: Other Engineering Material

Material Notes: Calcined Coke: Calcined coke is created by calcining petroleum coke calcined at a high temperature of 1,300 ? in an oxygen-free environment to mainly drive off moisture and volatile matter. The calcinations modifies the structure and composition of the raw material, and increases its density, mechanical strength, conductivity, chemical stability, and oxidation resistance.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.01 g/cc0.0726 lb/inĀ³YS/T 587.9
Volatiles <= 1.0 %<= 1.0 %mass fraction; YS/T 587.3 a
Ash <= 0.50 %<= 0.50 %mass fraction; YS/T 587.1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 43000 - 50000 ohm-cm43000 - 50000 ohm-cmof granules; YS/T 587.6
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %mass fraction; YS/T 587.2
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S <= 3.0 %<= 3.0 %mass fraction; Chapter 4 in GB/T 214

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB056 / 318598

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.