MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 15W-40 Exxon XD-3 Elite
Categories: Fluid; Lubricant

Material Notes: Exxon XD-3 Elite 15W-40 is a synthetic blend heavy duty diesel engine oil that provides the highest level of protection to modern, high performance diesel engines used in severe on and off highway applications. Exxon XD-3 Elite 15W-40 exhibits outstanding low temperature fluidity, high temperature viscosity retention, and piston deposit control. Exxon XD-3 Elite 15W-40 is highly recommended for use in all high performance diesel engines, including modern low emission engines.

Naturally aspirated and turbo-charged diesel powered engines; On-highway light and heavy duty trucking including, mixed fleets; Off-highway industries including: mining, construction, quarrying, and agriculture

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc
@Temperature 15.0 °C
0.0314 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 137137Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 119 cSt119 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.6 cSt15.6 cStASTM D445
Ash 1.3 %1.3 %Sulfated Ash, wt%; ASTM D874
 
Chemical PropertiesMetricEnglishComments
Total Base Number 1212mg KOH/g; ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -30.0 °C-22.0 °FASTM D97
Flash Point 228 °C442 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON006 / 75431

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.