MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade
Categories: Polymer; Thermoplastic

Material Notes: Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistance
Applications-sanitary products, electrical parts

Information provided by Global Polymers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 1.9 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.9 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393ASTM D785
Tensile Strength, Ultimate 80.0 MPa11600 psiASTM D638
Flexural Yield Strength 134 MPa19400 psiASTM D790
Flexural Modulus 3.834 GPa556.1 ksiASTM D790
Izod Impact, Notched 0.256 J/cm0.480 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C187 °FASTM D648
Vicat Softening Point 106 °C223 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Protective Coating PC-Fahrenheit™ High Temperature Epoxy
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance

PGLOBX12 / 42166

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.