MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals TBIR2249 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: TBIR: Trans-1,4-poly(butadiene-co-isoprene) rubber (TBIR), a new functional rubber material with excellent properties, is a solution to the compatibility problem of such common rubber as natural rubber, cis-1,4-polybutadiene rubber, and styrene-butadiene rubber. With improvement in the dispersion of fillers in the rubber mix, various types of rubber can deliver great performance. The rubber compound containing TBIR has a high green strength and great dimensional stability; the vulcanized rubber containing TBIR has high fatigue resistance and wear resistance, and low rolling resistance and heat generation.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %mass fraction, Acceptable product
 <= 5.0 %<= 5.0 %mass fraction, High-class product
Mooney Viscosity  46 - 52
@Temperature 100 °C
46 - 52
@Temperature 212 °F
ML(3+4), High-class product
 44 - 54
@Temperature 100 °C
44 - 54
@Temperature 212 °F
ML(3+4), Acceptable product
Ash <= 1.0 %<= 1.0 %mass fraction
 
Descriptive Properties
AppearanceWhite or light yellow granule/solid block
Content19-25%1,3-Butadiene, mole
Vulcanization characteristics1.5-4.5 dN-mFL
 10.5-16.5 dN-mFH
 10-15 minT50
 2.5-5.5 minT90
 4.5-8.5 minTs1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB069 / 318611

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.