Physical Properties | Original Value | Comments |
---|
Density | 0.970 g/cc @Temperature 100 °C |
| 0.997 g/cc @Temperature 50.0 °C |
| 1.002 g/cc @Temperature 100 °C |
| 1.009 g/cc @Temperature 0.000 °C |
| 1.024 g/cc @Temperature 50.0 °C |
| 1.03 g/cc @Temperature 50.0 °C |
| 1.036 g/cc @Temperature 0.000 °C |
| 1.039 g/cc @Temperature 100 °C |
| 1.057 g/cc @Temperature 100 °C |
| 1.06 g/cc @Temperature 50.0 °C |
| 1.072 g/cc @Temperature 0.000 °C |
| 1.074 g/cc @Temperature 100 °C |
| 1.078 g/cc @Temperature 50.0 °C |
| 1.09 g/cc @Temperature 0.000 °C |
| 1.097 g/cc @Temperature 50.0 °C |
| 1.108 g/cc @Temperature 100 °C |
| 1.109 g/cc @Temperature 0.000 °C |
| 1.135 g/cc @Temperature 50.0 °C |
| 1.142 g/cc @Temperature 100 °C |
| 1.147 g/cc @Temperature 0.000 °C |
| 1.174 g/cc @Temperature 50.0 °C |
| 1.178 g/cc @Temperature 100 °C |
| 1.187 g/cc @Temperature 0.000 °C |
| 1.215 g/cc @Temperature 50.0 °C |
| 1.216 g/cc @Temperature 100 °C |
| 1.229 g/cc @Temperature 0.000 °C |
| 1.237 g/cc @Temperature 100 °C |
| 1.258 g/cc @Temperature 50.0 °C |
| 1.259 g/cc @Temperature 100 °C |
| 1.274 g/cc @Temperature 0.000 °C |
| 1.28 g/cc @Temperature 50.0 °C |
| 1.298 g/cc @Temperature 0.000 °C |
| 1.311 g/cc @Temperature 100 °C |
| 1.322 g/cc @Temperature 0.000 °C |
| 1.351 g/cc @Temperature 50.0 °C |
| 1.373 g/cc @Temperature 0.000 °C |
| 1.376 g/cc @Temperature 100 °C |
| 1.402 g/cc @Temperature 50.0 °C |
| 1.40 - 1.45 g/cc @Temperature 20.0 °C |
| 1.43 g/cc @Temperature 0.000 °C |
| 1.457 g/cc @Temperature 50.0 °C |
| 1.463 g/cc @Temperature 100 °C |
| 1.492 g/cc @Temperature 0.000 °C |
pH | 1.0 - 1.4 |
Viscosity | 0.287 cP @Temperature 100 °C |
| 0.311 cP @Temperature 100 °C |
| 0.349 cP @Temperature 100 °C |
| 0.371 cP @Temperature 100 °C |
| 0.395 cP @Temperature 100 °C |
| 0.449 cP @Temperature 100 °C |
| 0.512 cP @Temperature 100 °C |
| 0.564 cP @Temperature 50.0 °C |
| 0.586 cP @Temperature 100 °C |
| 0.628 cP @Temperature 50.0 °C |
| 0.673 cP @Temperature 100 °C |
| 0.722 cP @Temperature 100 °C |
| 0.737 cP @Temperature 50.0 °C |
| 0.775 cP @Temperature 100 °C |
| 0.802 cP @Temperature 50.0 °C |
| 0.874 cP @Temperature 50.0 °C |
| 0.894 cP @Temperature 100 °C |
| 1.033 cP @Temperature 100 °C |
| 1.044 cP @Temperature 50.0 °C |
| 1.196 cP @Temperature 100 °C |
| 1.253 cP @Temperature 50.0 °C |
| 1.511 cP @Temperature 50.0 °C |
| 1.828 cP @Temperature 50.0 °C |
| 1.852 cP @Temperature 0.000 °C |
| 2.014 cP @Temperature 50.0 °C |
| 2.149 cP @Temperature 0.000 °C |
| 2.22 cP @Temperature 50.0 °C |
| 2.681 cP @Temperature 0.000 °C |
| 2.703 cP @Temperature 50.0 °C |
| 3.011 cP @Temperature 0.000 °C |
| 3.3 cP @Temperature 50.0 °C |
| 3.392 cP @Temperature 0.000 °C |
| 4.039 cP @Temperature 50.0 °C |
| 4.332 cP @Temperature 0.000 °C |
| 5.575 cP @Temperature 0.000 °C |
| 7.217 cP @Temperature 0.000 °C |
| 9.392 cP @Temperature 0.000 °C |
| 10.732 cP @Temperature 0.000 °C |
| 12.277 cP @Temperature 0.000 °C |
| 16.112 cP @Temperature 0.000 °C |
| 21.222 cP @Temperature 0.000 °C |
| 28.044 cP @Temperature 0.000 °C |
Molecular Weight | 162.2 g/mol |
|
Descriptive Properties |
---|
Color | red brown |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding