MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping

Automotive Specifications: Chrysler MS-DB590 CPN4660; Ford WSB-M4D734-A

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
Linear Mold Shrinkage 0.011 in/inASTM D955
 0.013 in/inASTM D955
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9515 seconds; ASTM D2240
Hardness, Shore D 4210 seconds; ASTM D2240
Tensile Strength, Yield 1100 psiType 1, 20 in/min; ASTM D638
 1490 psi2.0 in/min; ASTM D638
Tensile Stress at Strain 1220 psi
@Strain 100 %
2.0 in/min; ASTM D412
 1240 psi
@Strain 300 %
2.0 in/min; ASTM D412
Elongation at Break 140 %Type 1, 20 in/min; ASTM D412
 550 %2.0 in/min; ASTM D412
Elongation at Yield 16 %Type 1, 20 in/min; ASTM D638
Flexural Modulus 42100 psiASTM D790
Poissons Ratio 0.337
@Temperature -35.0 °C
ASTM D638
 0.363
@Temperature 85.0 °C
ASTM D638
 0.419
@Temperature 23.0 °C
ASTM D638
Izod Impact, Notched NB
@Temperature -40.0 °C
ASTM D624
Gardner Impact 300 in-lb
@Temperature -30.0 °C
ASTM D3029
Tensile Impact Strength 224 ft-lb/in²ASTM D1822
Tear Strength 63.8 kN/mDie C; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.0 µin/in-°F
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 65.0 µin/in-°F
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 145 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °FUnannealed; ASTM D648
Glass Transition Temp, Tg -68.6 °FDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Zone 1 330 - 370 °F
Zone 2 340 - 380 °F
Zone 3 350 - 390 °F
Zone 5 360 - 400 °F
Die Temperature 374 - 410 °F
Melt Temperature 370 - 410 °FProcessing Temperature
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive
Taiwan PU Corporation TPU-E95 General Grade, Extrusion Molding Polyester Base TPU
Spartech Formalloy TPR Thermoplastic Rubber Alloy Specialty Sheet
Polymax® Maxelast® C4800 TPE, Transparent

PTEKNP569 / 129642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.