MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Greene Tweed FLUORAZ® 797 Fluoroelastomer, FEPM
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known for its capabilities in high-temperature environments and its chemical resistance, Greene, Tweed`s Fluoraz has proven field performance in both dynamic and static applications.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6464After 70hrs @347°F in Stauffer 7700
 8080ASTM D2240
Hardness, Shore M 8383ASTM D2240
Tensile Strength at Break 14.5 MPa2100 psiAfter 70hrs @347°F in Stauffer 7700
 19.3 MPa2800 psiASTM D1414
Tensile Strength, Yield 3.86 MPa560 psi@50% Elongation; ASTM D1414
 9.136 MPa1325 psi@100% Elongation; ASTM D1414
Elongation at Break 225 %225 %ASTM D1414
 258.75 %258.75 %After 70hrs @347°F in Stauffer 7700
Coefficient of Friction 0.500.50ASTM D1894
Coefficient of Friction, Static 0.800.80ASTM D1894
Tear Strength Test 315315lb/in; ASTM D624 Die B
Compression Set 19 %
@Temperature 23.0 °C
19 %
@Temperature 73.4 °F
ASTM D395
 27 %
@Temperature 200 °C,
Time 79200 sec
27 %
@Temperature 392 °F,
Time 22.0 hour
at 25% deflection; ASTM D395
 40 %
@Temperature 200 °C,
Time 79200 sec
40 %
@Temperature 392 °F,
Time 22.0 hour
at 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -5.00 °C23.0 °F
Shrinkage 25 %
@Temperature 175 °C,
Time 252000 sec
25 %
@Temperature 347 °F,
Time 70.0 hour
in Stauffer 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM
Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM
Greene Tweed FLUORAZ® 790 Fluoroelastomer, FEPM
Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM

PGREEN41 / 42335

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.