MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Astaras Anviloy® Weld Rod
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.

Applications:

  • Repair cracked or broken dies
  • Reconstruction of outbreaks and washouts
  • Repair or enhance casting tools and cores
  • Armor, strengthen or re-coat areas exposed to high erosion or corrosion
  • Increase the resistance to thermal fatigue and heat checking
  • Increase erosion or corrosion resistance
  • Reduce the tendency to soldering

Astaras, Inc. purchased the entire Anviloy® business from CMW in 2014. Information provided by Astaras, Inc.

Key Words: Powder Metallurgy (P/M)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 1430 - 3410 °C
Solidus 1430 °C
Liquidus 3410 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 13.5 %
Nickel, Ni 26.5 %
Tungsten, W 60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
NAECO® ELKON® 100W Pure Tungsten
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy
AISI 1069 Steel Composition Spec (UNS G10690)
ASTM A500 Steel, grade C, shaped structural tubing

NCMW01 / 15873

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.