MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R plus 4105/40 HCR silicone rubbers are addition-curing, two part compounds (batch grades). The vulcanizates show excellent transparency and good to very good mechanical properties. Properly postcured vulcanizates of ELASTOSIL® R plus 4105/40 comply with BfR and FDA food contact regulations. The material also passes USP XXIII Class VI and ISO 10993 certification is available.

Application: ELASTOSIL® R plus 4105/40 is intended for fabrication of extruded articles that afford high transparency and very good tear resistance values.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 - 1.14 g/cc1.10 - 1.14 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240
Tensile Strength 11.0 MPa1600 psiASTM D412
Elongation at Break 950 %950 %ASTM D412
Tear Strength 28.0 kN/m160 plidie B; ASTM D 624
Compression Set 18 %
@Temperature 175 °C,
Time 79200 sec
18 %
@Temperature 347 °F,
Time 22.0 hour
WSTM 1114
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Transparent, but not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 165 °C
0.250 hour
@Temperature 329 °F
press cured, post cured 4 h/200 °C in ventilated air
Pot Life 480 min480 minWSTM 2299
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
AppearanceTransparentWSTM 1279

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® R 427/30 High Strength Silicone Base
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 25A, Non-Black Sulfur Cure
Shin-Etsu Silicones KE-2090-20A/B Self-adhesive LIMS Silicone
NuSil VersaSil 40 MED-4042 Silicone

PWACK9934 / 197533

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.