Varcum 29112 is a one-step crushed phenolic resin. APPLICATION: For use in metal coating formulations. FEATURES: - Exhibits sufficient flexibility without the addition of modifiers.
- Plasticizers can be utilized where maximum flexibility is required.
- Solvency characteristics permit the use of reasonable amounts of hydrocarbon solvents.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |