MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Availability: Asia Pacific

Features: Medium Impact Resistance

Uses: Electrical/Electronic Applications

Forms: Pellets

Processing Method: Injection Molding

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Melt Flow 17 g/10 min
@Load 21.6 kg,
Temperature 190 °C
17 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 57.8 MPa8390 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Izod Impact, Notched 0.390 J/cm0.730 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C
@Time 1800 sec
374 °F
@Time 0.500 hour
Congo Red; BS 2782
Vicat Softening Point 86.1 °C187 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fainplast Compounds MGS 75 Medical Flexible PVC, Injection Molding
Geon® Performance Solutions Vinyl Rigid Molding MR840 Polyvinyl Chloride, Rigid
Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding
Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding
Crystex Composites Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite

PTEKNP101 / 129182

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.