MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP30LP-2 High performance two part epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Very low viscosity
  • Superb optical clarity and light transmission properties
  • Exceptionally low shrinkage
  • Passes NASA low outgassing requirements
Master Bond EP30LP-2 is a two component, low viscosity epoxy resin system with superior optical clarity and light transmission for high performance bonding, sealing, coating, and encapsulating. It is formulated to cure readily at room temperature with a full cure being realized in 2-3 days. It cures more rapidly at elevated temperatures, 2-3 hours at 150-200°F. To optimize the properties, the recommended cure schedule is overnight at room temperature, followed by 2-3 hours at 150°F. It has a two to one mix ratio by weight or volume and contains no solvents or diluents. It has low shrinkage upon cure. EP30LP-2 has an impressive physical strength profile. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and many plastics. The cured material is also an outstanding electrical insulator. It is also relatively lower exothermic type epoxy, which allows it to be used for moderate sized potting and encapsulation applications. It has reasonably good chemical resistance to water, oils, fuels and hydraulic fluids. Its service temperature range is -60°F to +250°F. The color of Parts A and B is clear. EP30LP-2 is worthwhile to consder for electronic, electro-optic, optical as well as aerospace and vacuum type applications.

Product Advantages:

  • Easy handling: two to one by weight or volume
  • Very low viscosity, easy to apply for bonding or potting
  • Relatively long open time
  • Superb optical clarity; outstanding light transmission
  • Passes NASA low outgassing ASTM E595 specifications

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 100 - 400 cP100 - 400 cPPart B
 900 - 1600 cP900 - 1600 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85
Tensile Strength 55.2 - 62.1 MPa8000 - 9000 psi
Tensile Modulus 1.72 - 2.07 GPa250 - 300 ksi
Adhesive Bond Strength 16.5 - 17.9 MPa2400 - 2600 psilap shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.5
@Frequency 60 Hz
3.5
@Frequency 60 Hz
Dielectric Strength 17.3 kV/mm
@Thickness 3.17 mm
440 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 65.6 - 93.3 °C
2.00 - 3.00 hour
@Temperature 150 - 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Working Life 60.0 - 90.0 min60.0 - 90.0 minAfter mixing, 100 g batch
Shelf Life 1.00 Month1.00 MonthIn original unopened containers
 6.00 Month6.00 MonthIn syringes
 
Descriptive Properties
Cure scheduleovernight at 75°F followed by 2-3 hours at 150°FOptimum
Mixing Ratio2:1Parts A to B, by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM711 / 233768

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.