MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BYK Opibent® 1008 Layered Silicate
Categories: Ceramic; Clay

Material Notes: Description: Optibent® 1008 is a high-quality, activated and organically modified layered silicate product which creates thixotropic properties in dry-mix mortars. Optibent ® 1008 gives an excellent anti-settling effect. In plasters and renders sag resistance is improved and smoother workability properties are achieved since the silicate layers exert a lubricating effect during application

Applications:

  • EIFS
  • Plaster
  • Renders (base coats)

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/cc
pH 9.0 - 11
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 0.000 - 40.0 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 14 %
 
Descriptive Properties
Color/Formbeige free flowing powder
Sieve Residue<35%90 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Opibent® 1056 Layered Silicate
BYK Necowel FLE 55N Clay Additive
BYK Nanothix® B1490 Phylosilicate
BYK Mineral Colloid® MO Clay Additive
BYK Mineral Colloid® BP Bentonite

PBYK083 / 185080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.