MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Synthos SUNCHLON™ AD-312 Chlorinated Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SUNCHLON™ CPP resin is a thermoplastic resin produced by the chlorination of polypropylene. It is a nontoxic white or light yellow granular solid and can be easily soluble in organic solvents such as chlorinated hydrocarbons, toluene, butanone or other mixed solvent. And it has high hardness and good properties of wear-resistance, acid-resistance, salt water resistance and aging- resistance.

Application: Polypropylene (PP) is a resin which is widely used for film, molded products and other useful products. But due to its low polarity and high crystallinity, it is difficult to adhere. A better way to solve this problem is to use Chlorinated Polypropylene (CPP). SUNCHLON™ CPP is the best adhesive to PP, thermoplastic olefin elastomer (TPO) and other low surface energy substrate containing olefinic material. It is a high-performance adhesion promoter for paints, coating, inks and adhesives.
Its main usages are as follows:

  • Primer for plastic substrates for automobiles (bumpers, interior parts, wheel cap, etc)
  • Ink binder for film (gravure /silk-screen printings)
  • Adhesive for plastic molded containers and food wrapping film
  • Primer for construction, paint, adhesives

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 300 - 8000 cP20% in toluene
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 28 - 34 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW070 / 320101

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.