MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont™ 7723 Silver Conductor
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This silver conductor is fired at 500-540C and has excellent adhesion to Indium Tin Oxide coated Glass substrates for touch screen applications. Interconnection may be achieved through soldering, conductive adhesives and other means.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.82 g/cc
Solids Content 77 - 82 %
Filler Content 75 %Silver (Ag)
Particle Size 1.0 µm
Viscosity 85000 - 110000 cP
Thickness 15.0 - 20.0 microns
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.0030 ohm
 
Processing PropertiesOriginal ValueComments
Cure Time 600 sec
 
Descriptive Properties
Binder SystemProprietary
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesSoda lime glass, ITO coated glass, alumina and others
Solvent SystemTerpeniol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vibrantz Technologies CF 8463 Low-Temperature Sealing
Vibrantz Technologies CF 1417 Low-Temperature Sealing
Vibrantz Technologies CF 7567 Low-Temperature Sealing
Corning Macor® Machinable Glass Ceramic
Trelleborg Emerson & Cuming Eccobond® 286 Two-Component General Purpose Epoxy Adhesive

PFLEXCM46 / 179448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.