Synthetic, hydrophilic, amorphous silica, produced via flame hydrolysis. Standard product for industrial applications. Special features: White colloidal powder of high purity. Application HDK® V15A is applied as a thickening and thixotropic agent in silicone sealants. In comparison to HDK® V15 the product shows higher thickening efficiency. Information provided by Wacker Chemie AG. |