MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21TPFL-1 Two Component Low Viscosity Epoxy Polysulfide Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Polysulfide Sealant/Adhesive

Material Notes: Key Features:
  • High flexibility
  • First rate electrical insulator
  • Good chemical resistance
  • Cures at room temperature
Product Description: Master Bond EP21TPFL-1 is a two component, low viscosity epoxy polysulfide system, which upon curing, offers a highly special combination of flexibility and chemical resistance. EP21TPFL-1 has excellent resistance to a wide array of chemicals including water, gasoline, fuels, oils, hydrocarbons and hydraulic fluids. It has been formulated to cure readily at ambient temperatures. Unlike most two part epoxies, heat curing is not recommended. This system has a non-critical mix ratio of one to two, by weight or volume. EP21TPFL-1 has good physical strength and superior electrical insulation properties. This allows the system to be utilized in situations involving rigorous thermal cycling as well as thermal and mechanical shocks. It has very good adhesion to metals, ceramics, glass, and many rubbers and plastics. Since it is a first class insulator, with low viscosity as well as low exotherm, it is serviceable as a potting and encapsulation system. The service temperature range is -60°F to +250°F. The color of Part A is clear while Part B is brown. Polysulfide systems have been traditionally used for many years as fuel tank sealants, as well as for electrical connectors exposed to fuels, oils and lubricants, for many years. EP21TPFL-1 can also be used in aerospace, electronic and specialty OEM, among other applications, where this highly unusual combination of superb flexibility along with superior chemical resistance is desirable.

Product Advantages:

  • Convenient mixing: forgiving one to two mix ratio by weight or volume
  • Low viscosity enhances ease of application, compound flows evenly and smoothly; ideal for potting
  • Cures at ambient temperatures
  • 100% reactive — no volatiles emitted during curing
  • Outstanding flexibility with superior resistance to thermal cycling
  • Polysulfide type chemical resistance profile

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 700 - 1300 cPPart B
 2000 - 4000 cPmixed
 10000 - 15000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 50
Tensile Strength 1000 - 3000 psi
Elongation at Break >= 250 %
Adhesive Bond Strength 400 - 600 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.9
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 135 - 150 µm/m-°C
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 72.0 - 120 hour
Working Life 90.0 - 150 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio1:2 by weight or volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System
Abatron AboWeld 8104-13 Polysulfide-Epoxy Sealant and Caulk
Abatron AboWeld 8104-12 Polysulfide-Epoxy Sealant and Caulk

PMASTM841 / 185434

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.