MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer
Categories: Polymer; Film; Thermoplastic

Material Notes: Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers excellent adhesion properties to various substrates and has very good heat stability, making is suitable in extrusion coating and lamination applications.

Elvaloy® 2615 AC has a wide processing latitude in molding and extrusion equipment. It has good flow characteristics and lower melting range than low density polyethylene.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792 - ISO 1183
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238 - ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ASTM D2240 - ISO 868
Hardness, Shore D 31ASTM D2240 - ISO 868
Tensile Strength at Break 12.0 MPa500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 740 %500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0400 GPa1 mm/min; ASTM D638 - ISO 527-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 97.0 °CBy DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 58.0 °CA50 (10N); ASTM D1525 - ISO 306
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 150 °CExtrusion lamination and extrusion coating
 150 °CCast film
 150 °CBlown film
Middle Barrel Temperature 160 °CBlown film
 210 °CCast film
 220 °CExtrusion lamination
Front Barrel Temperature 170 °CBlown film
 250 °CCast film
 290 °CExtrusion lamination
Adapter Temperature 180 °CBlown film
 250 °CCast Film
 290 °CExtrusion lamination
Die Temperature 356 °FBlown film
 482 °FCast film
 554 °FExtrusion lamination
 
Descriptive Properties
EA-Content15 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
Dow Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Dow Entira® ASSD100 Ionomer Resin
DuPont Elvaloy® 2715 AC Ethylene and 15% Ethyl Acrylate Copolymer
Dow Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer

PDUPM061 / 33728

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.