MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chambroad Petrochemicals HMA-1 Durable High-modulus Asphalt
Categories: Other Engineering Material

Material Notes: Durable High-modulus Asphalt: The durable high-modulus modified asphalt is the product from the secondary deep processing of the hard asphalt produced with high-quality imported crude oil. The product features high stiffness modulus, great fatigue resistance, and excellent performance at lowtemperatures. In combination with the pavement design, it enables the reduction in the composite structure thickness by 39 cm, saving23,000 tons/km of stone. It is expected to increase the life of the pavement structure from 15 years to more than 35 years, and reducecarbon emissions by 50% in the whole life cycle. We cooperate with scientific research institutes and downstream customers to buildthe Zhanlin Expressway Demonstration Road, and promote the demonstration and application of a new generation of the expresswaypavement structure. It helps to reduce costs, improve quality, and increase efficiency for engineering construction, facilitates the rapiddevelopment of industrial chains such as expressway construction, maintenance, and new materials, powers Shandong’s highwayindustry for “Taking the Lead” in China and boosts China's strength in transportation. Appraised by the Shandong Society of Chemistry and Chemical Engineering, the technological achievements have reached theinternational advanced level, and won the Second Prize of the Shandong Society of Chemistry and Chemical Engineering for Scientificand Technological Achievements in 2021.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity <= 1000 cSt
@Temperature 175 °C
JTG E20/T 0625-2011
 
Mechanical PropertiesOriginal ValueComments
Penetration 25 - 35
@Load 0.100 kg,
Time 5.00 sec
JTG E20/T 0604-2011
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 230 °Copen cup; JTG E20/T 0611-2011
Ring & Ball Softening Point >= 70.0 °CJTG E20/T 0606-2011
 
Descriptive Properties
Ductility>20 cm10?, 5cm/min, JTG E20/T 0605-2011

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHAMB079 / 318621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.