MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plywood
Categories: Wood and Natural Products; Wood

Material Notes: Plywood is made of several thin layers, or 'plies' that are laminated together. The layer structure leads to more uniform properties than solid wood, since the effects of grain anisotropy are minimized. The properties of plywood vary with the quality of the constituent layers; typical values of sheathing grade are listed below.

Key Words: Timber, Lumber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.400 - 0.600 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4000 - 5000 psiparallel to face; ASTM D3500
Modulus of Rupture 7.00 - 10.0 ksiparallel to face; ASTM D3043
Flexural Modulus 8.20 - 10.3 GPaparallel to face; ASTM D3043
Compressive Strength 4500 - 6000 psiparallel to face; ASTM D3501
Shear Modulus 20.0 - 30.0 ksiin plane (rolling shear)
 85.0 - 110 ksithrough thickness (edgewise shear)
Shear Strength 0.250 - 0.300 ksiin plane (rolling shear)
 0.800 - 1.00 ksithrough thickness (edgewise shear
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.10 µm/m-°C
@Temperature 20.0 °C
parallel to face
Thermal Conductivity 0.760 - 1.02 BTU-in/hr-ft²-°Fat 12% moisture; depends on wood species
 
Descriptive Properties
Linear Hygroscopic Expansion< 0.020%30 - 90% RH

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Douglas-fir Plywood
Carbon-Core 10 mm+2.7 mm Lauan both sides Luan/Meranti Plywood Panels
Carbon-Core 25 mm+2.7 mm Lauan both sides Luan/Meranti Plywood Panels
AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)
AISI 4140 Steel, oil quenched, 540°C (1000°F) temper, 25 mm (1 in.) round

PTSPLY / 71376

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.