MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 220 Mobil DTE FM Series
Categories: Fluid; Lubricant

Material Notes: Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qualified as NSF H1 type lubricants and also comply with Title 21 CFR 178.3570 by the Food and Drug Administration (USA) for lubricants with incidental food contact. The lubricants are tasteless, odourless, premium quality lubricants formulated with non-toxic NSF/FDA food grade additives and base oils. The additive system provides good wear protection, excellent oxidation stability and protection against rust. They provide good system cleanliness, long oil/filter life, and optimum equipment protection. The Mobil DTE FM Series oils are excellent gear, bearing and circulating oils. They are also suitable for handling the critical requirements of hydraulic system components such as close clearance servo-valves and the high accuracy numerically controlled (NC) machine tools. These products meet the most rigorous performance requirements of a wide range of system and component manufacturers using various multi-metallurgy designs allowing a single product with outstanding performance characteristics. The Mobil DTE FM Series oils have high ratings in the FZG Gear Test demonstrating their excellent protection against wear and scuffing. This allows their use in systems other than hydraulics that may contain gears and bearings. The naturally high viscosity index of the base oils ensures outstanding performance over a wide temperature range.

Suitable for multi-service applications in the lubrication of machinery used in all food processing industries, fish processing and met packing plants; Excellent gear, bearing, circulating system and hydraulic oils; Compressors and vacuum pumps handling air and inert gasses; Air line lubricators; Systems requiring a high degree of load-carrying capability and anti-wear protection; Mobil DTE FM 220, 320 and 460 are recommended for freezer plants and for outdoor applications due to their low temperature properties and high temperature stability; Machines employing a wide range of components using various metallurgy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.854 g/cc
@Temperature 15.6 °C
ASTM D4.52
Viscosity Measurement 143Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 214.3 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 24.5 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.250 mm20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -21.0 °CASTM D97
Flash Point 246 °CASTM D92
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Copper Strip Corrosion1A3 hrs @ 100°C
FZG Gear Test, DIN 51534, Fail Stage12+
Rust Prevention, Distilled WaterpassASTM D665A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON108 / 75533

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.