MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Unifrax XPE® MP Substrate Support Mat
Categories: Ceramic

Material Notes: XPE®-MP is a multipurpose, third-generation support mat system developed by Unifrax specifically for mechanical support and insulation of ceramic substrates used in diesel and gasoline emission control devices.

This product combines the unique performance characteristics of both non-intumescent and vermiculite-based mats in the same product.

At low operating temperatures (less than 350°C), the product will behave as a non-intumescent mat, relying on its spring-like ceramic fiber matrix to provide the holding force required for the system. At temperatures above 350°C, a second feature of the product is activated. Small amounts of vermiculite particles within the fiber matrix compensate for thermal gap expansion of the shell, thus providing additional holding force to the ceramic substrate.

As a result, XPE-MP is an ideal solution for a wide range of emission control devices, including large diesel oxidation catalysts (DOC), diesel particulate filters (DPF), selective catalyst reduction units (SCR) as well as gasoline oxidation catalysts, including E-85 underbody converters.

Support mat long-term durability is one of the critical issues involved in assuring a robust design for high-efficiency emission control systems. A variety of mechanisms are currently available to improve long-term cold holding performance and erosion resistance, but they may add extra production steps and cost to the system.

XPE-ME has been designed to provide robust performance without the need for wire mesh ring protection (for erosion) or heat treatment for additional holding force at low temperatures.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Loss On Ignition >= 6.5 %>= 6.5 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 0.100 MPa>= 14.5 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.120 W/m-K
@Temperature 650 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 
Descriptive Properties
Binder Content (%)5-10
Fiberfrax® Fibers (%)60-70
Vermiculite (%)21-31

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO)
Borealis HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE2591 High Density Polyethylene Powder for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Unifrax XPE® NV Substrate Support Mat

CUNIF134 / 97906

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.