MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gabriel Versamid® 100 Polyamide Resin
Categories: Polymer; Thermoset

Material Notes: Versamid® products have proven to be superior coatings resins in many applications, such as industrial maintenance and marine coatings, high-performance architectural paints and high-solids and conventional coatings.

Advantages:

  • Highly resistant to chemical and water corrosion
  • Strong adhesion to a variety of substrates
  • Long pot life
  • Lower sensitivity to substrate impurities
  • Most comply with FDA regulations
Principal Applications: Solvent-based maintenance coatings; used with solid epoxy resins

Comments/Advantages: Fast cure, good chemical resistance

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 g/cc0.0351 lb/in³
Solids Content 100 %100 %Theo
Viscosity 3000 - 5000 cP
@Temperature 120 °C
3000 - 5000 cP
@Temperature 248 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 9.0<= 9.0
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 min1.50 hourTack Free Time; 3 wet mils
 2880 min48.0 hourThrough Cure; 3 wet mils
Pot Life 960 min960 min60% solids
 
Descriptive Properties
Amine Value85-95[mg KOH/g]
Chemical TypePolyamide
PHR for Max DSC, Tg100190 EEW Epoxy; With 525 EEW Epoxy Resin (Solid basis)
Theo Amine Hydrogen Equl Wt.525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGABR971 / 230672

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.