MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 639 Mobil SHC 600 Series
Categories: Fluid; Lubricant

Material Notes: Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are formulated from synthesised, wax-free hydrocarbon base fluids. The combination of a naturally high viscosity index and a unique, proprietary, additive system enables these products to provide outstanding performance in extreme service applications at high and low temperatures, well beyond the capabilities of mineral oils. These products are resistant to mechanical shear, even in heavily loaded gear and high shear bearing applications, so that there is virtually no loss of viscosity. The Mobil SHC 600 Series products have low traction coefficients, which derive from the molecular structure of the base stocks used. This results in low fluid friction in the load zone of non-conforming surfaces such as gears and rolling contact bearings. Low fluid friction produces lower operating temperatures and improved gear efficiency, which translates into reduced power consumption. It also results in extended parts life and allows for more economical equipment design. The base oils used in the Mobil SHC 600 Series have outstanding response to antioxidant additives resulting in superior resistance to oxidation and sludging, especially at high temperatures. The additive combination used in these oils also provides exceptional resistance to rusting and corrosion, very good antiwear, demulsibility, foam control and air release properties, as well as multimetal compatibility. The Mobil SHC 600 Series oils are also compatible with the same seal and other construction materials used in equipment normally lubricated with mineral oils. While initially recognised as a high temperature problem solver, these products are now used in many industrial applications because of the range of benefits they offer.

While Mobil SHC 600 Series are compatible with mineral oil based products, admixture may detract from their performance. Consequently it is recommended that before changing a system to one of the Mobil SHC 600 Series, it should be thoroughly cleaned out and flushed to achieve the maximum performance benefits. The Mobil SHC 600 Series oils are compatible with the following seal materials: fluorocarbon, polyacrylate, polyurethane ether, some silicone, ethylene/acrylic, chlorinated polyethylene, polysulfide, and some nitrile rubbers. There is the potential for substantial variations in the elastomers being used today. For best results, consult your equipment supplier, seal manufacturer, or your local Mobil representative to verify compatibility. Mobil SHC 600 Series lubricants are recommended for use in a wide variety of gear and bearing applications where high or low temperatures are encountered or where operating temperatures or bulk oil temperatures are such that conventional lubricants give unsatisfactory life, or where improved efficiency is needed. They are particularly effective in applications where the maintenance costs of component replacement, system cleaning and lubricant changes are high. Specific applications include: Filled for life gearboxes, especially high ratio/ low-efficiency worm gears; Remotely located gearboxes, where oil change-out is difficult; Low temperature applications, such as ski lifts where seasonal oil changes can be avoided; Mixer roll bearings and roll neck bearings where high temperatures are encountered; Plastic calendars; Severe centrifuge applications, including marine centrifuges; Railroad A/C Traction Drives; Mobil SHC 625*, 627, 629 and 630 are suitable for Oil Flooded Rotary Screw Compressors compressing natural gas, field gas gathering, CO2 and other process gasses used in the natural gas industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.870 g/cc
@Temperature 15.0 °C
0.870 g/cc
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 164164Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 933 cSt933 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 79.5 cSt79.5 cStASTM D445
Oxidative Stability 1750 hour1750 hourRotating Bomb Oxidation Test (RBOT); ASTM D2272
 >= 10000 hour>= 10000 hourTurbine Oil Stability Test (TOST); ASTM D943
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °FASTM D97
Flash Point 270 °C518 °FASTM D92
 
Descriptive Properties
Colororange
Copper Strip Corrosion, ASTM D1301B24 hrs @ 121°C
Demulsibility Time (min)40to 3 mL emulsion @ 82°C
Foam Sequence I, ASTM D9450/0
Foam Sequence II, ASTM D89320/0
Foam Sequence III, ASTM D8930/0
FZG Scuffing Test, A/16.6/90, Fail Stage13+DIN 51534
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Synfoam® LG-20 Syntactic Foam
Solvay Chemicals IXOL® M 125
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam
J6 Polymers JFOAM™ S-1200 Engineered Specialty Foam

WEXXON125 / 75550

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.