MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nylon

(Viewing data as-entered. Click here to return)
Nylacast Polypropylene (PP)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Light weight copolymer material with high impact, stress cracking, and chemical resistance. Has great flexibility and toughness at low temperatures with low moisture intake

Information provided by Nylacast Ltd.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccMethod A; ISO 1183:1987
Water Absorption 0.2 %
@Time 86400 sec
Immersion; ISO 62:1999
Moisture Absorption at Equilibrium 0.10 %ISO 62:1999
Water Absorption at Saturation 0.9 %Immersion; ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ISO 868:2003
Tensile Strength 26.0 MPaType 1B, 50 mm/min; ISO 527-1/2:1993
Elongation at Break 7.0 %Type 1B, 50 mm/min; ISO 527-1/2:1993
Tensile Modulus 2700 MPaType 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 80.0 MPa1.5 mm/min; ISO 178:2001
Flexural Modulus 1200 MPa1.5 mm/min; ISO 178:2001
Compressive Strength 110 MPaType B, 5 mm/min; ISO 604:2002
Compressive Modulus 2600 MPaType A, 5 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 7.20 kJ/m²Type A; ISO 180:2000
Charpy Impact, Notched 0.700 J/cm²ISO 180
Coefficient of Friction, Dynamic 0.25
@Pressure 1.75 MPa
3.14 m/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250:1969-01
Dielectric Strength 16.5 kV/mmIEC 60243-1:1998-01
Dissipation Factor 0.0050
@Frequency 100 Hz
IEC 60250:1969-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Thermal Conductivity 0.310 W/m-KISO 8301
Melting Point 170 °C
Maximum Service Temperature, Air 140 °CIntermittent
 82.0 °C
@Time 1.80e+7 sec
Continuous
Deflection Temperature at 0.46 MPa (66 psi) 110 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CISO 75/A
Glass Transition Temp, Tg -60.0 °CISO 11359-2
Flammability, UL94 HBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorWhite/Black/Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global EPP POM C Acetal Copolymer
Mitsubishi Chemical Advanced Materials Proteus™ Copolymer PP Natural Polypropylene
Syensqo (Solvay Specialty Polymers) Solef® 1008 PVDF Homopolymer
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade
Imerys NYGLOS® 4W STO105 Wollastonite in Polypropylene

PNYLAC14 / 197403

Nylon

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.