MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials Minlon® IG38C1 BK434 PA66-(MD+GF)38  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: 38% Mineral/Glass Reinforced Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³DAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
DAM; Sim. to ISO 62
 5.4 %
@Thickness 2.00 mm
5.4 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.40 %
@Thickness 2.00 mm
1.40 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.0 MPa10400 psi50% RH; ISO 527-1/-2
 120 MPa17400 psiDAM; ISO 527-1/-2
Elongation at Break 2.5 %2.5 %DAM; ISO 527-1/-2
 4.0 %4.0 %50% RH; ISO 527-1/-2
Tensile Modulus 5.00 GPa725 ksi50% RH; ISO 527-1/-2
 7.50 GPa1090 ksiDAM; ISO 527-1/-2
Flexural Modulus 7.00 GPa1020 ksiDAM; ISO 178
Poissons Ratio 0.340.34DAM; ISO 527-1/-2
 0.350.3550%RH; ISO 527-1/-2
Izod Impact, Notched (ISO) 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
Izod Impact, Unnotched (ISO)  3.80 kJ/m²
@Temperature -40.0 °C
1.81 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.300 J/cm²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FDAM; ISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 305 °C545 - 581 °FInjection
 295 °C563 °FInjection Optimum
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FInjection Optimum
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Part Marking CodePA66-(MD+GF)38ISO 11469
ProcessingInjection Molding
Regional AvailabilityNorth America
 South and Central America
Resin IdentificationPA66-(MD+GF)38ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural

PDSX5254 / 197894

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.