MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AISI Type 304HN Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: High Nitrogen 304 stainless steel. Austenitic Cr-Ni stainless steel. Nitrogen provides higher tensile and tensile yield strength without diminishing ductility, corrosion resistance, or nonmagnetic properties. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion.

Applications: Aircraft and Aerospace components, marine components, high temperature components, pressure vessels, pump components, welded tubing, forged fittings, pipe flanges, and valves.

Weldability: Can be brazed and welded using common methods. Grain-boundary carbide precipitation can occur in heat-affected zones (HAZ). Annealing will restore corrosion resistance to the weldment.

Key Words: aisi304, AISI 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, T304HN, 304HN, 304 HN, UNS S30452, ASME S240 (XM-21), ASTM A240 (XM-21), ASTM A276 (XM-21), 18-8, high nitrogen
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 725 MPa
Tensile Strength, Yield 415 MPa
@Strain 0.2 %
Elongation at Break 50 %
Reduction of Area 75 %
Modulus of Elasticity 197 GPaestimated from comparison of similar stainless steels.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.9 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Melting Point 1400 - 1455 °C
Solidus 1400 °C
Liquidus 1455 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 18 - 20 %
Iron, Fe 66 - 73.8 %as balance
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 10.5 %
Nitrogen, N 0.16 - 0.30 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
AISI Type 304L Stainless Steel
AISI Type 304HN Stainless Steel, Annealed Bar
AISI Type 304N Stainless Steel
304 Stainless Steel (UNS S30400); Cold Finished and Annealed Bar

MQ304HN / 12675

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.