MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® HDPE A4046 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: SABIC® HDPE A4046 is a medium density HDPE and is typically used for the production of PE-Xb compounds. The additive package has been optimized for the silane grafting process. The typical application of these is the manufacture of PEX pipes for hot and cold water and central heating. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccASTM D1505
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 31.0 MPaSpeed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Tensile Strength, Yield 22.0 MPaSpeed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Elongation at Break 200 %Speed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Tensile Modulus 800 MPaSpeed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 186 J/gDIN 53765
Melting Point 130 °CDIN 53765
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CISO 75-2
Vicat Softening Point 121 °Cat 10 N (VST/A); Compression moulding of test specimen according to ISO 1872-2,Conditioning of test specimen: temp. 23 °C, relative humidity 50 %, 24 hours; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10876 / 244343

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.