MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips 5570 LDPE High Clarity, Medium Impact Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Resin Type: Homopolymer

Characteristics: Good Optical Properties, Good Impact Strength, Excellent Processability, High Antiblock and Low Slip

Applications:Baby Bottle Liners

Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.

Film properties below based on film thickness of 31.8 µm.

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 1.3 g/10 min1.3 g/10 minCondition E; ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Secant Modulus, MD 0.210 GPa30.5 ksiASTM D882
Secant Modulus, TD 0.230 GPa33.4 ksiASTM D882
Coefficient of Friction 0.700.70ASTM D1894
Dart Drop 2.50 g/micron63.5 g/milF50; 1.5 in. dart/26 in. drop height; ASTM D 1709
 
Optical PropertiesMetricEnglishComments
Haze 6.5 %6.5 %ASTM D2457
Gloss 65 %65 %at 45°. ASTM D 2457
 105 %105 %at 60°. ASTM D 2457
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 °C399 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
Celanese 7110 LDPE polymer for medical
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene

PCHEVVA8 / 20504

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.