MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Rynite® FR530 BK507 PET-GF30FR(17)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: 30% Glass Reinforced, Flame Retardant, Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183
Water Absorption 0.75 %
@Thickness 2.00 mm
DS; Sim. to ISO 62
Moisture Absorption 0.150 %
@Thickness 2.00 mm
DS; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527-1/-2
Elongation at Break 1.9 %ISO 527-1/-2
Tensile Modulus 11300 MPaISO 527-1/-2
Flexural Strength 200 MPaISO 178
Flexural Modulus 10500 MPaISO 178
Poissons Ratio 0.33
Charpy Impact Unnotched 30.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.1
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 39.0 kV/mmDS; IEC 60243-1
Dissipation Factor 0.0127
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.0309
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 200 VIEC 60112
 250 - 399 VPLC 2; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°CISO 11359-1/-2
 17.0 µm/m-°C
@Temperature 55.0 - 160 °C
ISO 11359-1/-2
 19.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 96.0 µm/m-°CISO 11359-1/-2
 68.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 125 µm/m-°C
@Temperature 55.0 - 160 °C
ISO 11359-1/-2
Melting Point 252 °C10°C/min; ISO 11357-1/-3
Hot Ball Pressure Test 230 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 243 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °CISO 75-1/-2
Glass Transition Temp, Tg 90.0 °C10°C/min; ISO 11357-1/-2
UL RTI, Electrical 155 °C
@Thickness 0.400 mm
UL 746B
 155 °C
@Thickness 0.750 mm
UL 746B
 155 °C
@Thickness 1.50 mm
UL 746B
 155 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical with Impact 155 °C
@Thickness 0.400 mm
UL 746B
 155 °C
@Thickness 0.750 mm
UL 746B
 155 °C
@Thickness 1.50 mm
UL 746B
 155 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 155 °C
@Thickness 0.400 mm
UL 746B
 155 °C
@Thickness 0.750 mm
UL 746B
 155 °C
@Thickness 1.50 mm
UL 746B
 155 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.350 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 5VA
@Thickness 1.50 mm
IEC 60695-11-20
Oxygen Index 33 %ISO 4589-1/-2
Glow Wire Ignition Temperature 800 °C
@Thickness 0.750 mm
IEC 60695-2-13
 800 °C
@Thickness 1.50 mm
IEC 60695-2-13
 850 °C
@Thickness 2.00 mm
IEC 60695-2-13
 925 °C
@Thickness 3.00 mm
IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °COptimum, Injection
 270 - 290 °CRange, Injection
Mold Temperature 110 °COptimum, Injection
 100 - 120 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %Injection
Hold Pressure >= 80.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassDNIISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-GF30FR(17)<ISO 11469
PolymerPET-GF30 FR
Processing Hold Pressure Time (s/mm)4Injection
Railway classificationR23DIN 53236
Railway classification ratingHL1EN 45545-2
Resin IdentificationPET-GF30FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Rynite® FR530 NC010 PET-GF30FR(17)
Celanese Rynite® 530 BK503 PET-GF30
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Conditioned)
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled

PDSX5272 / 197912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.