MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
CMT Materials METAPOR® HD 100 AL Air Permeable Material
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Metal Filled

Material Notes: METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design considerations for prototype and production thermoform tools. In contrast to sintered materials, the pores do not close off after machining allowing excellent definition and surface quality.

METAPHOR®-HD 100 AL is the high density grade of the material that is recommended for use in applications where the surface characteristics of the finished part are critical. HD 100 AL is specially formulated to have a smooth surface yielding better transparency on clear or translucent parts. The material is also recommended for use with acrylics and in twin-sheet applications.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 118.5 lb/ft³
Porosity 16 %Total porosity (by volume)
Pore Size 0.500 milMean pore diameter
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
Flexural Strength 6327 psi
Flexural Modulus 1335 ksi
Impact 11Unspecified Impact Test (kJ/m2)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.8 µin/in-°F
@Temperature 25.0 - 125 °C
Thermal Conductivity 20.5 W/m-K
@Temperature 100 °C
Maximum Service Temperature, Air 226 °FMartens Dimensional Stability

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMT Materials METAPOR® BF 100 AL Air Permeable Material
CMT Materials METAPOR® HD 210 AL Air Permeable Material
CMT Materials PROTOBLOCK Air Permeable Prototype Tooling Material
Goodfellow Polyacrylamide/acrylate Hydrogel
Poraver Metapor®

PCMT021 / 93149

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.