QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 230F is exceptionally good where highly detailed parts and mold flexibility are required. QM 230F has a shorter work life than QM 230 and QM 230 Clear. Material complies with FDA indirect food contact regulation CFR 177.2600 Key Features: - Low viscosity
- Fast demold time
- Casting resin resistance
- Excellent flexibility
Main Applications:- Molds for architectural replication
- Molds for polyester, polyurethane and epoxy resin castings
- Molds for technical articles and prototype
- Molds for furniture and picture frame replication
- Candy and other food molds
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017
|